tina@xinjuchengmim.com
Contact Us
Phone: 0755-27196558
Mobile: 13714218668
Email: tina@xinjuchengmim.com
MIM process
The process combines the design flexibility of injection molding with the high strength and monolithic integrity of precision metals, delivering a low-cost solution for highly complex geometric components.
The process is divided into four distinct manufacturing steps—mixing, forming, degreasing, and sintering—to produce the components, with surface treatment determined on a case-by-case basis according to the product’s characteristics.
|
|
(1) Mixing materialsThe mixing process is carried out in a dedicated mixing unit, where the mixture is heated to a specific temperature to melt the binder. In most cases, mechanical mixing is employed until the metal powder particles are uniformly coated with the binder; the resulting blend is then extruded into rod‑shaped strands and cut into pellets—referred to as feedstock—which can be directly fed into an injection molding machine for injection molding. |
|
|
(ii) MoldingThe equipment and technology used in injection molding are similar to those of plastic injection molding. Granular raw material is fed into the machine, heated, and injected into the mold cavity under high pressure. However, when designing the mold cavity dimensions, it is essential to account for the shrinkage rate of the product during the sintering process. The shrinkage rate for each metallic material is well‑known and highly precise. |
|
|
(3) DefattingDebinding is the process of removing the binder from a green part. This process is typically carried out in several steps. The vast majority of the binder is removed prior to sintering, while the residual binder serves to support the part as it enters the sintering furnace. Currently, Zhucheng Company operates an integrated degreasing and sintering machine, which automatically performs both the degreasing and sintering of formed components within a single piece of equipment. |
|
|
(4) SinteringThe degreased component is placed in a sintering furnace with precisely controlled high temperature and pressure. Under a protective gas atmosphere, the component is slowly heated to remove any residual binder. After the binder has been completely removed, the component is heated to a very high temperature, causing the inter-particle pores to disappear as the particles fuse together. The high densification of MIM parts is achieved through elevated sintering temperatures and extended sintering times, thereby significantly enhancing and improving the mechanical properties of the material. |